US20080153234A1 - Flash memory device and method of manufacturing the same - Google Patents
Flash memory device and method of manufacturing the same Download PDFInfo
- Publication number
- US20080153234A1 US20080153234A1 US12/041,932 US4193208A US2008153234A1 US 20080153234 A1 US20080153234 A1 US 20080153234A1 US 4193208 A US4193208 A US 4193208A US 2008153234 A1 US2008153234 A1 US 2008153234A1
- Authority
- US
- United States
- Prior art keywords
- forming
- polysilicon layer
- layer
- groove
- polysilicon
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Abandoned
Abstract
A non-volatile memory device includes a semiconductor substrate having an active region defined by isolation films that extend along a first direction. A control gate line extends along in a second direction perpendicular to the first direction. First and second floating gates are formed on the active region and below the control gate line. An island conductive line is formed between the first and second floating gates and within the isolation films. The island conductive line extends along the first direction and is configured to receive a voltage in order to prevent interference between the first and second floating gates.
Description
- The present invention generally relates to semiconductor memory devices, and more particularly, to a flash memory device and a method of manufacturing the same, in which an interference phenomenon can be reduced.
- As the level of integration of NAND flash memories becomes high, the influence of cells adjacent to a programmed cell on the programmed cell is gradually increased.
- Capacitance exists between cells that are adjacent to each other in a bit line direction (or x direction), a word line direction (or y direction), and a xy direction. The capacitance gradually increases as the distance between the cells becomes smaller as the level of integration of devices becomes higher. More particularly, the capacitance is significantly increased when the cells shrink in the x direction.
- As a result, as the coupling ratio is reduced, the program speed is lowered and the interference phenomenon is increased.
- The term “interference phenomenon” refers to a phenomenon in which if a neighboring cell to a to-be read cell is to be programmed, a threshold voltage of a cell, which is higher than an actual threshold voltage, is read due to the capacitance effect of an adjacently programmed cell during the read operation of a next cell because of variation in the charge of the floating gates of the neighboring cell. In this case, the charge itself of the floating gate of the to-be read cell is not changed, but the status of an actual cell looks distorted due to variation in the status of the neighboring cell.
- This distortion phenomenon widens the distributions of cells and, therefore, makes it difficult to control the cells. More particularly, the influence is significantly greater in multi-level cells having a small cell distribution margin than in single-level cells.
- To improve the cell uniformity, it is necessary to reduce the interference phenomenon.
- An embodiment of the present invention provides a flash memory device and a method of manufacturing the same, in which the interference phenomenon can be reduced.
- Another embodiment of the present invention provides a flash memory device and a method of manufacturing the same, in which an operational malfunction can be prevented through the reduction of the cell distributions.
- Still another embodiment of the present invention provides a flash memory device and a method of manufacturing the same, in which multi-level cells having a small cell distribution margin can be fabricated through the reduction of the cell distributions.
- Another embodiment of the present invention provides a flash memory device and a method of manufacturing the same, in which the program speed can be enhanced.
- Still another embodiment of the present invention provides a flash memory device and a method of manufacturing the same, in which devices of a high integration level can be fabricated by reducing the interference phenomenon serving to limit the high integration.
- According to one embodiment of the present invention, a flash memory device comprises a memory cell, the memory cell including a semiconductor substrate having active regions defined by isolation films arranged in one direction, control gate lines arranged in a direction perpendicular to the isolation films, floating gates formed on the active regions below the control gate lines, and island polysilicon lines formed within the isolation films in the same direction as that of the isolation films and applied with a voltage in order to prevent the interference between neighboring floating gates with the isolation films therebetween.
- According to another embodiment of the present invention, a method of manufacturing a flash memory device comprises etching a semiconductor substrate resulting in a plurality of isolation trenches arranged in one direction; forming a first insulating layer on the semiconductor substrate, the first insulating layer having grooves within the isolation trenches of the semiconductor substrate; forming island polysilicon lines at the bottoms of the grooves; forming a second insulating layer so that the isolation trenches are completely buried, and stripping the second insulating layer and the first insulating layer so that the semiconductor substrate is exposed, forming isolation films within the isolation trenches; forming tunnel oxide films on active regions defined by the isolation films; forming floating gates on the tunnel oxide films; and forming a control gate on the entire structure with a dielectric layer intervened therebetween.
- According to another embodiment of the present invention, a method of manufacturing a flash memory device comprises forming a tunnel oxide film and a first polysilicon layer on a semiconductor substrate; etching the first polysilicon layer, the tunnel oxide film, and a part of the semiconductor substrate, resulting in a plurality of isolation trenches arranged in one direction; forming a first insulating layer on the entire structure, the first insulating layer having grooves within the isolation trenches; forming island polysilicon lines at the bottoms of the grooves; forming a second insulating layer so that the isolation trenches are fully buried, and stripping the second insulating layer and the first insulating layer so that the first polysilicon layer is exposed, thereby forming isolation films within the isolation trenches; forming second polysilicon layers on the first polysilicon layer and the isolation films adjacent to the first polysilicon layer, thereby forming floating gates respectively having lamination film of the first polysilicon layer and the second polysilicon layer; and forming a control gate on the entire structure including the floating gates with a dielectric layer intervened therebetween.
- In another embodiment, a non-volatile memory device includes a semiconductor substrate having an active region defined by isolation films that extend along a first direction. A control gate line extends along in a second direction perpendicular to the first direction. First and second floating gates are formed on the active region and below the control gate line. An island conductive line is formed between the first and second floating gates and within the isolation films. The island conductive line extends along the first direction and is configured to receive a voltage in order to prevent interference between the first and second floating gates.
- In another embodiment, a method of manufacturing a non-volatile memory device includes etching a semiconductor to form a trench; providing a first insulating layer within the first trench without completely filling the trench, so that a groove is formed within the trench; providing a conductive layer within the groove, so that the conductive layer remains only at a lower portion of the groove to define an island conductive line; forming a second insulating layer within the groove and over the island conductive line, wherein the first and second insulating layers define an isolation structure, the island conductive line being provided within the isolation structure; forming first and second floating gates on first and second sides of the isolation structure, so that the isolation structure is provided between the first and second floating gates; and forming a control gate line over the first and second floating gates.
- In yet another embodiment, a method of manufacturing a non-volatile memory device includes forming a tunnel oxide film and a first polysilicon layer on a semiconductor substrate; etching the first polysilicon layer, the tunnel oxide film, and a portion of the semiconductor substrate to form an isolation trench arranged in a first direction; forming a first insulating layer within the isolation trench to form a groove defined by the first insulating layer; forming an island polysilicon line at a lower portion of the groove; forming a second insulating layer within the groove and over the island polysilicon line to define an isolation structure, the isolation structure including the first and second insulation layers, the island polysilicon layer being provided within the isolation structure; forming second polysilicon layer on the first polysilicon layer to form a floating gate having a lamination film of the first polysilicon layer and the second polysilicon layer; and forming a control gate over the second polysilicon layer.
- A more complete appreciation of the invention will be readily apparent as the same becomes better understood by reference to the following detailed description when considered in conjunction with the accompanying drawings in which like reference symbols indicate the same or similar components, wherein:
-
FIG. 1 is a view illustrating the construction of a flash memory device according to an embodiment of the present invention; -
FIGS. 2A to 2F are cross-sectional views illustrating a method of manufacturing a flash memory cell according to an embodiment of the present invention; and -
FIGS. 3A to 3J are cross-sectional views illustrating a method of manufacturing a flash memory cell according to another embodiment of the present invention. -
FIG. 1 is a view illustrating the construction of a flash memory device according to an embodiment of the present invention. - Referring to
FIG. 1 , a flash memory cell according to an embodiment of the present invention includes asemiconductor substrate 10 in which active regions 12 are defined byisolation films 11 arranged in a first direction,control gate lines 14 arranged in a second direction perpendicular to the first direction, floatinggates 13 formed on the active region 12 below thecontrol gate lines 14, andisland polysilicon lines 15 formed within theisolation films 11 along the first direction as with theisolation films 11 and applied with a voltage in order to prevent the interference between thefloating gates 13. - Though not shown in the drawing, tunnel oxide films are disposed between the
floating gates 13 and thesemiconductor substrate 10 and gate dielectric films are disposed between thefloating gates 13 and thecontrol gate lines 14. - The
island polysilicon lines 15 are interconnected at the edge region of the memory cell so that theisland polysilicon lines 15 can be applied with the same voltage. - Meanwhile, switching
circuit 20 for supplying a voltage to theisland polysilicon lines 15 is included in a peripheral region for driving the memory cell. - In some embodiments, the
switching circuit 20 is a MOS transistor that is turned on during the program, erase, and read operations of the memory cell. Theswitching transistor 20 has one end to which an input voltage Vin is input and the other end connected to theisland polysilicon lines 15, so that when the memory cell is driven, Vin can be transmitted to theisland polysilicon lines 15. - The input voltage Vin may have different voltage values depending on the operating status of a memory cell so that there is no potential between the
island polysilicon lines 15 and the floating gates of neighboring cells. - In the program operation, a pass voltage applied to a control gate of a non-selected memory cell is used as Vin, and in the erase operation, no voltage is applied so that the
island polysilicon lines 15 are floated. Meanwhile, in the read operation, a voltage of 0V is used as Vin. -
FIGS. 2A to 2F are cross-sectional views illustrating a method of manufacturing a flash memory cell according one embodiment of the present invention.FIGS. 2A to 2F illustrate an example in which the present invention is applied to a typical Shallow Trench Isolation (STI) structure. - Referring first to
FIG. 2A , apad oxide film 31 and apad nitride film 32 are sequentially formed on asemiconductor substrate 30. Thepad nitride film 32, thepad oxide film 31, and a part of thesemiconductor substrate 30 are etched by a photolithography process, forming a plurality ofisolation trenches 33 extending along one direction. The etched depth of thesemiconductor substrate 30 may be set to about 2000 Å. - Referring to
FIG. 2B , thepad nitride film 32 and thepad oxide film 31 are removed. A High Density Plasma (HDP) oxide film is then deposited on the entire structure to form a firstinsulating layer 34. In this case, the thickness of the first insulatinglayer 34 is properly controlled so that agroove 70 is formed within each of thetrenches 33 in such a manner that thetrenches 33 are not fully filled. Thegroove 70 has a valley-like shape in the present embodiment. - A
polysilicon layer 35 is deposited on the entire structure. Thepolysilicon layer 35 is etched back, so that it remains only at a lower portion of thegroove 70 as shown inFIG. 2C , thereby formingisland polysilicon lines 35 a. - Thereafter, a HDP oxide film is deposited on the entire structure, forming a second
insulating layer 36. Chemical Mechanical Polishing (CMP) is performed on the secondinsulating layer 36 and the firstinsulating layer 34 so that thesemiconductor substrate 30 is exposed, as shown inFIG. 2D . Accordingly,isolation films 37 respectively having the first and second insulatinglayers island polysilicon line 35 a at the bottom are formed. - Referring to
FIG. 2E , polysilicon layers 39 for floating gates are formed on the active region defined by theisolation films 37 and theisolation films 37 adjacent to the active regions.Tunnel oxide films 38 are between the polysilicon layers 39 and thesubstrate 30. - Referring to
FIG. 2F , a dielectric layer 40 and apolysilicon layer 41 for a control gate are sequentially formed on the entire structure. - Though not shown in the drawings, the
polysilicon layer 41, the dielectric layer 40, thepolysilicon layer 39, and thetunnel oxide film 38 are etched in a direction orthogonal to the direction in which theisolation films 37 are arranged, forming a stack gate having the tunnel oxide film, the floating gates, the dielectric layer, and the control gate. Subsequent processes are performed to complete the flash memory cell. -
FIGS. 3A to 3J are cross-sectional views illustrating a method of manufacturing a flash memory cell according to another embodiment of the present invention.FIGS. 3A to 3J illustrate an example in which the present invention is applied to a Self-Aligned Shallow Trench Isolation (SA-STI) structure. - Referring to
FIG. 3A , atunnel oxide film 51, afirst polysilicon layer 52, and ahard mask film 53 are sequentially formed on asemiconductor substrate 50. Thehard mask film 53 may be formed using a nitride film. - A first photoresist PR1 is then formed on the entire structure. The first photoresist PR1 is patterned to open a field region, as shown in
FIG. 3B . Thehard mask film 53 is patterned by an etch process using the patterned first photoresist PR1 as a mask. - Thereafter, as shown in
FIG. 3C , the first photoresist PR1 is stripped in order to prevent etch failure by the first photoresist PR1 in a subsequent etch process. - A plurality of
isolation trenches 54 is formed by etching thefirst polysilicon layer 52, thetunnel oxide film 51, and a portion of thesemiconductor substrate 50 using the patternedhard mask film 53 as a mask. The isolation trenches are formed to extend along a first direction. The etched depth of thesemiconductor substrate 50 may be set to about 2000 Å. - Referring to
FIG. 3D , a HDP oxide film is deposited on the entire structure to form a first insulatinglayer 55. Agroove 72 is formed by controlling the thickness of the first insulatinglayer 55. - A
second polysilicon layer 56 is deposited on the entire structure. Thesecond polysilicon layer 56 is etched back so that thesecond polysilicon layer 56 remains only at a lower portion of eachgroove 72, as shown inFIG. 3E , thereby forming anisland polysilicon line 56 a. A HDP oxide film is then deposited on the entire structure so that thetrenches 54 are fully filled, thus forming a second insulatinglayer 57. - Referring to
FIG. 3F , the second insulatinglayer 57 and the first insulatinglayer 55 are stripped by CMP so that thefirst polysilicon layer 52 is exposed, thereby formingisolation films 58. Each of theisolation films 58 has the first and second insulatinglayers island polysilicon line 56 a at the bottom of thegroove 72. - Referring to
FIG. 3G , athird polysilicon layer 59 is formed on the entire structure. A second photoresist PR2 is coated on thethird polysilicon layer 59 as shown inFIG. 3H . The second photoresist PR2 is patterned so that thethird polysilicon layer 59 on theisolation films 58 is exposed. - Referring to
FIG. 3I , thethird polysilicon layer 59 is etched using the patterned second photoresist PR2 as a mask, forming floatinggate patterns 60. Each floatinggate 60 has a lamination film of thefirst polysilicon layer 52 and thethird polysilicon layer 59. The second photoresist PR2 is stripped from thethird polysilicon layer 59. - Referring to
FIG. 3J , adielectric layer 61 and apolysilicon layer 62 for a control gate are formed on the entire structure. - Thereafter, though not shown in the drawings, the
polysilicon layer 62 for the control gate, thedielectric layer 61, the floating gate thepatterns 60 and thetunnel oxide film 51 are etched in a direction orthogonal to the direction in which theisolation films 58 are arranged, thereby forming a stack gate having the tunnel oxide film, the floating gates, the dielectric layer and the control gate. Subsequent processes are performed to complete the flash memory cell. As described above, the embodiments of the present invention has one or more of the following advantages. First, since the interference phenomenon can be reduced, the limit to the level of integration of devices due to the interference phenomenon can be overcome. It is therefore possible to enhance the level of integration of devices. Second, since the interference phenomenon can be reduced, cell distributions can be reduced and device operation failure can be prevented accordingly. Third, since the cell distributions can be reduced, multi-level cells having a small cell distribution margin can be fabricated. Fourth, since the interference phenomenon can be reduced, the coupling ratio can be increased and the program speed can be enhanced. - While the invention has been described in connection with what is presently considered to be practical exemplary embodiments, it is to be understood that the invention is not limited to the disclosed embodiments, but, on the contrary, is intended to cover various modifications and equivalent arrangements included within the spirit and scope of the appended claims.
Claims (9)
1. A method of manufacturing a non-volatile memory device, the method comprising:
etching a semiconductor to form a trench;
providing a first insulating layer within the first trench without completely filling the trench, so that a groove is formed within the trench;
providing a conductive layer within the groove, so that the conductive layer remains only at a lower portion of the groove to define an island conductive line;
forming a second insulating layer within the groove and over the island conductive line, wherein the first and second insulating layers define an isolation structure, the island conductive line being provided within the isolation structure;
forming first and second floating gates on first and second sides of the isolation structure, so that the isolation structure is provided between the first and second floating gates; and
forming a control gate line over the first and second floating gates.
2. The method as claimed in claim 1 , wherein the first insulating layer and the second insulating layer are formed using a high density plasma oxide film.
3. The method as claimed in claim 1 , wherein the providing-a-conductive-layer-within-the-groove step includes:
providing a polysilicon layer within the groove and over the first insulating layer; and
etching the polysilicon layer until the polysilicon layer remains only at a lower portion of the groove.
4. A method of manufacturing a non-volatile memory device, the method comprising:
forming a tunnel oxide film and a first polysilicon layer on a semiconductor substrate;
etching the first polysilicon layer, the tunnel oxide film, and a portion of the semiconductor substrate to form an isolation trench arranged in a first direction;
forming a first insulating layer within the isolation trench to form a groove defined by the first insulating layer;
forming an island polysilicon line at a lower portion of the groove;
forming a second insulating layer within the groove and over the island polysilicon line to define an isolation structure, the isolation structure including the first and second insulation layers, the island polysilicon layer being provided within the isolation structure;
forming second polysilicon layer on the first polysilicon layer to form a floating gate having a lamination film of the first polysilicon layer and the second polysilicon layer; and
forming a control gate over the second polysilicon layer.
5. The method as claimed in claim 4 , wherein the first insulating layer and the second insulating layer are formed using a high density plasma oxide film.
6. The method as claimed in claim 4 , wherein forming island polysilicon line comprises:
forming a polysilicon layer on the entire surface of the semiconductor substrate in which the first insulating layer is formed; and
etching back the polysilicon layer so that the polysilicon layer remains only at the lower portion of the groove.
7. The method as claimed in claim 4 , wherein the etching of the first polysilicon layer, the tunnel oxide film, and the semiconductor substrate is performed using a hard mask film as a mask.
8. The method as claimed in claim 4 , the isolation trench has a depth of about 2000 Å.
9. The method as claimed in claim 7 , wherein the hard mask film is a nitride film.