Prior art keywords
film
substrate
rotating
light signal
fiber
Prior art date
Application number
PCT/US1993/012609
Other languages
French (fr)
Inventor
Wallace T. Y. Tang
Original Assignee
Tang Wallace T Y
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Tang Wallace T Y filed Critical Tang Wallace T Y
Priority to JP51799495A priority Critical patent/JP3993888B2/en
Priority to PCT/US1993/012609 priority patent/WO1995018353A1/en
Publication of WO1995018353A1 publication Critical patent/WO1995018353A1/en

Links

Classifications

    • GPHYSICS
    • G01MEASURING; TESTING
    • G01BMEASURING LENGTH, THICKNESS OR SIMILAR LINEAR DIMENSIONS; MEASURING ANGLES; MEASURING AREAS; MEASURING IRREGULARITIES OF SURFACES OR CONTOURS
    • G01B11/00Measuring arrangements characterised by the use of optical techniques
    • G01B11/02Measuring arrangements characterised by the use of optical techniques for measuring length, width or thickness
    • G01B11/06Measuring arrangements characterised by the use of optical techniques for measuring length, width or thickness for measuring thickness ; e.g. of sheet material
    • G01B11/0616Measuring arrangements characterised by the use of optical techniques for measuring length, width or thickness for measuring thickness ; e.g. of sheet material of coating
    • G01B11/0683Measuring arrangements characterised by the use of optical techniques for measuring length, width or thickness for measuring thickness ; e.g. of sheet material of coating measurement during deposition or removal of the layer

Abstract

A technique and apparatus is disclosed for the optical monitoring and measurement of a thin film (11) undergoing thickness and other changes while it is rotating (10). An optical signal is routed from the monitored area through the axis of rotation (6) and decoupled from the monitored rotating area. The signal can then be analyzed (12) to determine an endpoint to the planarization process. The invention utilizes interferometric and spectrophotometric optical measurement techniques for the in situ, real-time endpoint control of chemical-mechanical polishing planarization in the fabrication of semiconductor or various optical devices.

Description


  
 



   METHOD AND APPARATUS FOR MONITORING THIN FILMS
FIELD OF THE INVENTION
 The present invention is directed to a technique and apparatus for the optical monitoring and measurement of a surface undergoing rotation, particularly for in situ, real-time monitoring of any thin film undergoing rotation and simultaneous dimensional changes.



  It is particularly useful in the field of wafer planarization for producing wafers of extreme flatness and uniformity that are desirable in the production of semiconductor and integrated circuits.



  BACKGROUND OF THE INVENTION
 As microelectronic device dimensions continue to shrink, patterning problems increasingly hinder integrated circuit and semiconductor device fabrication. Semiconductor device fabrication often requires extremely planar surfaces and thin films of precise thicknesses. The surfaces requiring planarization and thickness control in semiconductor devices include areas or layers of dielectric material (such as Si02) on the surface of semi conducting materials and other device pattern layers. The insulating dielectric layers and other device layers need to be extremely planar because irregularities and rough topography lead to fabrication problems, including Depth of Focus budget (hereafter
DOF) problems.

   Since an irregularity in the surface can cause part of the surface to be out of focus at a particular distance between the optical system and the wafer, errors in pattern formations can occur. Also, the thickness of layers needs to be precisely controlled because variations in thickness may affect the electrical properties of the layers and adjacent device patterns, particularly in the interconnections between the different layers of microelectronic devices.



   The precise control of layer thickness is also crucial in semiconductor device fabrication. In VLSI technology, certain layers of multi-layer devices are generally electrically interconnected. These layers are also typically insulated from various levels by thin layers of insulating material such as sio2.



  In order to interconnect the device layers, contact holes are often formed in the insulating layers to provide electrical access there  between. If the insulating layer is too thick, the layers may not connect, if the layer is too thin, the hole formation process may damage the underlying device layer.



   Due to the various inadequacies of other planarization methods (such as spin-on-glass and etch back), Chemical/Mechanical
Polishing (hereafter CMP) planarization machines and other lapping machines have been developed and employed to provide planar surfaces for semiconductor device fabrication. Generally, CMP is a technique of planarizing wafers through the use of a polishing pad attached to a rotating table. The wafer is held by a chuck above a polishing pad which rotates on a spindle. The wafer is pressed downward against the polishing pad. The nap of the rotating pad removes bits of the film layer, thereby planarizing the surface.



   A solution of pH controlled fluid and colloidal silica particles called slurry flows between the pad and the wafer to remove material from the polishing area and to enhance the planarization of the wafer surface.



   A typical method of determining the endpoint of CMP and lapping machines is to measure the amount of time needed to planarize standard wafer (s), and then to process the remaining wafers for a similar amount of time. In practice, this process is very inefficient because it is very difficult to determine the precise rate of film removal, as polishing conditions and the polishing pad change from wafer to wafer over time. As a result, it is often necessary to inspect the wafers individually after planarization, which is time-consuming and expensive. Thus, the CMP process could be significantly improved by introducing an in situ, real-time measurement and control system.



   The ability to monitor and control the CMP process has been directly and indirectly addressed by several techniques. One method is based on measuring capacitance (U. S. Patent No.



  5,081,421). The theory behind this method is that the electrical capacitance of the wafer changes as the wafer surface is planarized. The two primary drawbacks of the method are its limited accuracy and its pattern dependency. Its accuracy can be compromised by the patterns of underlying layers which may also affect the capacitance of the entire system.



   One direct method has been proposed which uses laser light to  make interferometric readings on the polished side (front side) of a section of the wafer which overhangs the polishing pad (U. S.



  Patent No. 5,081,796). The disadvantages of this system are that it requires substantial modification of the conventional CMP process since part of the wafer must overhang the edge of the polishing pad, leading to polishing uniformity problems, and also, the monitored spot on the rotating wafer must be coordinated with the apparatus underneath the wafer overhang.



   An indirect method of monitoring CMP has been developed which senses the change in friction between the wafer and the polishing surface (U. S. Patent No. 5,036,015). The change in friction may be produced when, for instance, an oxide coating of the wafer is removed and a harder material is contacted by the polishing pad.



  The accuracy of the method suffers from variations in changing pad conditions. In addition, use of the method may be limited by the need to sense the friction generated by different materials.



   Another indirect method of monitoring CMP has been developed utilizing the conductivity of the slurry during polishing (U. S.



  Patent No. 4,793,895). When metal layers are exposed during the
CMP process, the electrical resistivity of the slurry and wafer changes due to the exposed metal on the wafer surface. The obvious drawback of this method is that it requires having exposed metal surfaces for monitoring. This is not possible for most types of polishing situations.



   Another indirect method of monitoring CMP has been developed utilizing the waste slurry off the pad during planarization (U. S.



  Patent No. 4,879,258).



   Certain materials are imbedded in the dielectric layer and monitored as they are planarized and fall off the polishing pad.



  The obvious drawbacks to this method include the time delay between planarization and when the slurry reaches the edge of the pad (estimated to be approximately 30 seconds) and also the low levels of sensitivity and signal noise introduced by the materials left over from the previous wafers. This method is not an active, real-time method.



   These and other endpoint detection techniques do not offer effective and accurate control of the CMP process in an in situ, real-time manner. These schemes either compromise the accuracy of the endpoint detection and/or require significant  alterations of the CMP process.



  BRIEF DESCRIPTION OF THE FIGURES
 Fig. 1 is a side view of a representative semiconductor device with a device pattern on a substrate of semi conductive material and a thick, unplanarized dielectric layer over the pattern and substrate.



   Fig. 2 illustrates the semiconductor device of Fig. 1 after the dielectric layer has undergone CMP planarization.



   Fig. 3 is a side view of a rotating coupler fitted with fiberoptic cable.



   Fig. 4 is a side view representation of the fiber-optic embodiment of the present invention integrated with a CMP assembly.



  The fiber-optic apparatus is pictured in both a front side and a back side approach.



   Fig. 5 shows another embodiment of the present invention utilizing a light source which transmits light in the direction of the wafer, where it is reflected off the wafer's surface and the reflection is monitored by a photodetector which converts the light signal to an electrical signal. The electrical signal can be relayed to an analyzer after passing through an electrical slip ring.



   Fig. 6 illustrates a wafer-holding chuck shown in Fig. 4, wherein air has been pumped into a cavity above the wafer to compensate for loss of pressure against the back of the wafer where holes are located.



  SUMMARY OF THE INVENTION
 An object of the present invention is to avoid the abovementioned problems by allowing for the monitoring of a region of a film on a substrate undergoing thickness changes, thus enabling endpoint detection in an in situ, real-time manner. In addition, if the monitored region is sufficiently small, a spot on the wafer can be dedicated for endpoint purposes. The dedicated endpoint spot can remove signal problems associated with the layer's topology, patterns, and multiple film layers.



   The present invention thus provides an apparatus and method for the optical illumination and monitoring of a section on a thin film layer undergoing dimensional changes. Light from a light source  is transmitted to a monitoring area on the layer, preferably through the back side of the substrate, and relayed back to an analyzer which evaluates changes in thickness of the substrate based on interferometric, spectrophotometric, and/or absorption changes.



   In a preferred embodiment, the light signal is advantageously measured from the back side of the substrate, which facilitates implementation since the monitored region of the wafer and the monitoring apparatus do not need to be timed and coordinated during the process.



  DETAILED DESCRIPTION OF THE INVENTION
 In one embodiment, the present invention is a method of monitoring the thickness change of a film on a substrate comprising illuminating a section of the film through the back side (the side which is not being processed) of the substrate, measuring a light signal returning from the illuminated section, and determining change in thickness of the film on a substrate based on the measured light signal. Thickness change can be determined by an analyzer, which analyzes interferometric, spectrophotometric, absorption, and/or other optical changes in the measured light signal. Optionally, if the substrate is undergoing rotation, the method further comprises the step of relaying the light signal to a rotating coupler which links the signal to an analyzer.



   Another embodiment of the present invention is a method of monitoring the change in thickness of a film on a substrate comprising illuminating a section of the film from the front side (i. e., the side being polished) of the substrate, measuring a light signal returning from the illuminated section, and relaying the light signal to a rotating coupler which connects to an analyzer, and monitoring thickness change with the analyzer, which analyzes interferometric, spectrophotometric, absorption, and/or other optical changes in the measured light signal.



   Another embodiment of the present invention is an apparatus for monitoring thickness change in a film on a substrate comprising a light source which illuminates a section of the film from either the front side or back side of the substrate to generate a light signal, means for detecting the light signal, means for analyzing the light signal, a rotating coupler for relaying the light signal  from the illuminated section to the means for analyzing the light signal, and optionally one or more focusing lenses.



   Preferably, the apparatus comprises
 (i) a bifurcated fiber-optic cable having a common leg and two bifurcated legs,
 (ii) a rotating fiber-optic cable with two ends,
 (iii) a light source,
 (iv) means for analyzing a light signal, and
 (v) a rotating coupler having a stationary end and a rotating end.
 wherein the first bifurcated leg of the bifurcated fiber-optic cable is connected to the light source, the second bifurcated leg is connected to the means for analyzing a light signal, and the common leg is connected to the stationary end of the rotating coupler,
 and wherein one end of the rotating fiber-optic cable is connected to the rotating end of the rotating coupler and the other end is held in close proximity to the film on a substrate undergoing processing.



   "Close proximity"includes any distance between the end of the rotating fiber-optic cable and the film on the substrate that is close enough to permit effective illumination of the monitored area of the film and effective reception of the returning light signal.



  A preferred distance is less than or equal to about 1 cm.



   The rotating fiber-optic cable serves both to transmit light from the light source to the illuminated section and to transmit the returning light signal on its way back from the illuminated section. Light from the light source travels down the first bifurcated leg of the bifurcated fiber-optic cable and passes through the rotating coupler down the rotating fiber-optic cable to illuminate the film on a substrate. The returning light signal is relayed by the second bifurcated leg of the bifurcated fiberoptic cable to the analyzer. In addition, more than one section of the film on a substrate can be monitored at a time by using multiple legs of rotating fiber-optic cables which pass through one or more rotating couplers.



   Preferably, the fiber-optic cable comprises multiple optic fibers bundled together. However, the fiber-optic cable may comprise a single fiber. Alternatively, it may be a combination  of bundled fiber-optic cable and single fiber-optic cable.



  Alternatively, it may be multiple fiber-optic cables bundled together.



   The term"substrate"includes any insulating, conductive, and semi conductive materials known in the art. Preferred substrates are wafers such as silicon wafers, gallium-arsenide wafers, and silicon on insulator (SOI) wafers.



   The term"film on a substrates includes various dielectric layers known in the art, such as Si02, metal layers such as tungsten and aluminum, and various other films such as silicon films found on the substrate as defined above. The films also include resist layers.



   The film undergoing thickness change, for example, may be a film on a substrate in a chemical mechanical polishing (CMP) process, a chemical vapor deposition process, a resist development process, a post-exposure bake, a spin coating process, or a plasma etching process. In the CMP embodiment, the film is located at the interface of the substrate and the polishing pad.



   The term"light source"includes any source of light capable of illuminating a film on a substrate in the range of about 200 to about 11,000 nanometers in wavelength. If the light signal is measured from the back side of the substrate, the wavelength is preferably between about 1,000 and about 11,000 nanometers. A preferred back side wavelength is 1,300 nanometers. If the light signal is measured from the front side, then the wavelength is preferably between about 200 and about 11,000 nanometers. A preferred front side wavelength is 632.8 nanometers. Preferably, the section of the film on the substrate is continuously illuminated by the light source, although illumination can be at timed intervals.



   Suitable means for analyzing the light signal, or"analyzers," include photodetectors, interferometers, spectrophotometers, and other devices known in the art for measuring interferometric, spectrophotometric, absorption, and/or other optical changes.



   Suitable rotating couplers include any couplers known in the art for coupling a rotating member to a non-rotating member provided that light is permitted to pass between the ends of the two members. Such couplers are disclosed, for example, in U. S.



  Patent Nos. 4,398,791 and 4,436,367. Preferably, the means for  coupling the rotating fiber-optic cable to the bifurcated fiberoptic cable which is not rotating comprises a rotating member which attaches to one end of the rotating fiber-optic cable. The rotating member is fitted into a stationary member of the rotating coupler which is attached to the common leg of the bifurcated fiber-optic cable. The coupler is designed such that the end of the rotating fiber-optic cable is held in close proximity, preferably less than 1 cm, to the common leg of the bifurcated fiber-optic cable, thereby permitting light to pass between the two ends. Optionally, the cable ends can be fitted with focusing lenses to enhance signal transmission.



   The rotating coupler can be replaced with other types of couplers, including off-axis fiber-optic couplers, electrical slip rings, or a combination of the aforementioned couplers, or with other means of signal rotation decoupling.



   Typical CMP machines in which the methods and apparatus of the present invention can be used are those produced by R. Howard
Strasbaugh, Inc. in San Luis Obispo, California; Westech Systems,
Inc. in Phoenix, Arizona; and Cybeq Systems in Menlo Park,
California.



   Figs. 1 and 2 illustrate CMP planarization of a semiconductor device wafer. In Fig. 1 is shown a representative semiconductor device, which includes a dielectric layer such as Si02,1, deposited on the surface of a device pattern, 2, formed on a silicon wafer substrate, 3. The dielectric layer may be formed in a manner such as chemical vapor deposition (CVD) of oxide, spinon-glass, or by other means. Fig. 2 shows the wafer of Fig. 1, but with the dielectric layer, 1, planarized to a preselected thickness after CMP. The device pattern, 2, and the wafer substrate, 3, are relatively unchanged in this process.



   Fig. 3 is a side view representation of a preferred embodiment of the optical rotating coupler apparatus. Fig. 3 shows a bifurcated fiber-optic cable, 4, one bifurcated leg of which connects to a light source, 7, and another bifurcated leg of which connects to a photodetector, 8, which in turn is connected to signal conditioning electronics and a computer processing and control system (not shown). The common leg of the bifurcated fiber-optic cable, 4, connects to an optical rotating coupler, 5.



  A rotating fiber-optic cable, 6, extends from the rotating coupler  to the area of the wafer substrate to be monitored. The fiberoptic cables, 4 and 6, may be either single fiber or bundled fiber types.



  Also, it is possible to use several fiber-optic cables or fibers instead of one cable or fiber. Also, it is possible to make a hybrid single fiber and bundled fiber cable embodiment, e. g., cable 4 is single fiber and cable 6 is bundled cable. Focusing lenses are not necessary at the monitoring end of cable 6 if the cable is fixed securely and closely enough to the monitoring area of the wafer substrate. Preferably, the distance between the end of cable 6 and the wafer substrate is less than 1 cm.



   Fig. 4 is a side view representation of a typical CMP planarizer or lapping machine adapted with the apparatus shown in
Fig. 3. The apparatus may be set up in the planarizer from a back side approach with 4,5, and 6, or from a front side approach with 4', 5', and 6'. Only one of the approaches, either back side or front side, is needed at any one time for effective monitoring.



  In Fig. 4, the wafer holding-chuck and spindle, 12, is shown integrated with a rotating coupler, 5, for the back side approach.



  The bifurcated fiber-optic cable, 4, is fed into the spindle, 12, and connected to the stationary portion of the rotating coupler, 5, as shown in Fig. 3. The rotating fiber-optic cable, 6, is fed down the spindle to the monitored area of the wafer, 11, which monitored area is optionally a pattern less area such as a clear area or die or which is optionally an area having a pattern. The wafer, 11, is held to the chuck by a mounting pad or"fixture" which is generally attached to the chuck by a chemical adhesive.



  The fixture is often composed of a base matrix held together by a polyurethane surface layer. The outer surface which holds and presses against the back of the wafer, grips the wafer, and also provides uniform support for the wafer.



   In the other embodiment shown in Fig. 4, the rotating table base, 10, and platen, 9, which holds the polishing pad is shown integrated with a rotating coupler, 5', for a front side approach to the wafer. The bifurcated fiber-optic cable, 4', is fed into the rotating table base, 10, and connected to the stationary portion of the rotating coupler, 5'. The rotating fiber-optic cable, 6', connected to the rotating shaft of the rotating coupler, 5', is adjacent to the monitoring area of the wafer. As the polishing pad attached to the platen, 9, is generally perforated,  the end of the fiber-optic cable, 6', can be embedded in one of the holes. Translucent slurry solution flows in between the polishing pad and the wafer, scattering most visible light wavelengths.



  Optionally, signal enhancement means can be used to compensate for slurry scattering effects of different light wavelengths. In the preferred embodiment, the source light for the front side method is 632.8 nanometer wavelength light, a wavelength balancing the concerns of light signal transmission through the slurry, and also accuracy of measurement. The rotating fiber-optic cable, 6', embedded in the polishing pad must transmit and receive the interference signal when it is positioned over the measurement area on the wafer, 11. This is coordinated so that the monitoring optics pass over the monitored area on the wafer using ordinary skill in the art.



   Fig. 5 illustrates the use of an electrical slip ring assembly.



  A light source, 14, transmits light to a point on the wafer, 11, which causes the light to reflect in the direction of the photodetector or other light-monitoring electronics, 13, which convert the light signal into an electrical signal. The electrical signal may then be passed on to an analyzer, 12, and finally, to an electrical slip ring, 15, where it is decoupled from rotation and passed on to other analyzers which monitor the progress of CMP.



   Fig. 6 illustrates a wafer-holding chuck and spindle, 12, wherein the rotating fiber-optic cable, 6, has been routed from the coupler, 5, through the wafer-holding chuck, 12, to a point behind the wafer, 11, during the CMP process. If the pad or"fixture" which holds the wafer does not allow the passage of light, then it can be perforated to provide an optical access to the wafer. In order to compensate for the loss of pressure against the wafer at the point of optical access, air may optionally be pumped into the cavity to press against the wafer and compensate for the loss of pressure. Alternatively, if the fixture is able to transmit light, then the perforation for optical access is not necessary.



   While the invention has been described in detail and with reference to specific embodiments thereof, it will be apparent to one skilled in the art that various changes and modifications can be made therein without departing from the spirit and scope of the invention.
  

Claims

I claim: 1. A method of monitoring thickness change in a film on a substrate comprising the steps of illuminating a section of the film through the back side of the substrate, measuring a light signal returning from the illuminated section, and determining thickness change based on the measured light signal.
2. A method according to claim 1, wherein the substrate is undergoing rotation and the light signal is passed through a rotating coupler before it is measured.
3. A method according to claim 1, wherein the illuminated section of the film is pattern less.
4. A method according to claim 1, wherein the illuminated section of the film contains a pattern.
5. A method according to claim 1, wherein the film is undergoing a process selected from the group consisting of chemical mechanical polishing, chemical vapor deposition, resist development, post-exposure bake, spin coating, and plasma etching.
6. A method according to claim 1, wherein the illuminated section of the film is illuminated by light having a wavelength between about 1,000 and about 11,000 nanometers.
7. A method of monitoring thickness change in a film on a substrate undergoing rotation comprising the steps of illuminating a section of the film through the back side or from the front side of the substrate, measuring a light signal returning from the illuminated section with at least one photodetector undergoing the same rotation as the substrate, converting the light signal to an electrical signal, passing the electrical signal through an electrical slip ring and determining thickness change based on the electrical signal.
8. A method according to claim 7, wherein the film is undergoing a process selected from the group consisting of chemical mechanical polishing, chemical vapor deposition, resist development, post-exposure bake, spin coating, and plasma etching.
9. A method according to claim 7, wherein the illuminated section of the film is illuminated by light having a wavelength between about 1,000 and about 11,000 nanometers.
10. A method according to claim 7, wherein the illuminated section of the film is pattern less.
11. A method according to claim 7, wherein the illuminated section of the film contains a pattern.
12. A method of monitoring thickness change in a film on a substrate undergoing rotation comprising the steps of illuminating a section of the film from the front side of the substrate, measuring a reflected light signal returning from the illuminated section with at least one photodetector undergoing the same rotation as the substrate, passing the reflected light signal through a rotating coupler which connects to an analyzer and monitoring thickness change based on the measured light signal.
13. A method according to claim 12, wherein the film is undergoing a process selected from the group consisting of chemical mechanical polishing, chemical vapor deposition. resist development, post-exposure bake, spin coating, and plasma etching.
14. A method according to claim 12, wherein the illuminated section of the film is illuminated by light having a wavelength between about 200 and about 11,000 nanometers.
15. A method according to claim 12, wherein the illuminated section of the film is pattern less.
16. A method according to claim 12, wherein the illuminated section of the film contains a pattern.
17. An apparatus for monitoring thickness change in a film on a substrate comprising (i) a bifurcated fiber-optic cable having a common leg and two bifurcated legs, (ii) a rotating fiber-optic cable with two ends, (iii) a light source, (iv) means for analyzing a light signal, and (v) a rotating coupler having a stationary end and a rotating end, wherein the first bifurcated leg of the bifurcated fiber-optic cable is connected to the light source, the second bifurcated leg is connected to the means for analyzing a light signal, and the common leg is connected to the stationary end of the rotating coupler, and wherein one end of the rotating fiber-optic cable is connected to the rotating end of the rotating coupler and the other end is held in close proximity to the substrate.
18. An apparatus according to claim 17, wherein said other end of the rotating fiber-optic cable is held less than about 1 cm away from the substrate.
19. In a chemical mechanical polishing device for planarizing a film on a substrate, the improvement comprising (i) a bifurcated fiber-optic cable having a common leg and two bifurcated legs, (ii) a rotating fiber-optic cable with two ends, (iii) a light source, (iv) means for analyzing a light signal, and (v) a rotating coupler having a stationary end and a rotating end, wherein the first bifurcated leg of the bifurcated fiber-optic cable is connected to the light source, the second bifurcated leg is connected to the means for analyzing a light signal, and the common leg is connected to the stationary end of the rotating coupler, and wherein one end of the rotating fiber-optic cable is connected to the rotating end of the rotating coupler and the other end is held in close proximity to the substrate undergoing chemical mechanical polishing.
20. The device according to claim 19, wherein said other end of the rotating fiber-optic cable is held less than about 1 cm away from the substrate.
21. A method of monitoring thickness change in a film on a substrate comprising the steps of illuminating a section of the film through the back side of the substrate, measuring a reflected light signal returning from the illuminated section, and determining thickness change based on interferometric, spectrophotometric, or adsorption changes in the reflected light signal.
22. A method according to claim 1 wherein the substrate is undergoing rotation and/or translation.
PCT/US1993/012609 1993-12-28 1993-12-28 Method and apparatus for monitoring thin films WO1995018353A1 (en)

Priority Applications (2)

Application Number Priority Date Filing Date Title
JP51799495A JP3993888B2 (en) 1993-12-28 1993-12-28 Method and apparatus for monitoring thin films
PCT/US1993/012609 WO1995018353A1 (en) 1993-12-28 1993-12-28 Method and apparatus for monitoring thin films

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
PCT/US1993/012609 WO1995018353A1 (en) 1993-12-28 1993-12-28 Method and apparatus for monitoring thin films

Publications (1)

Publication Number Publication Date
WO1995018353A1 true WO1995018353A1 (en) 1995-07-06

Family

ID=22237334

Family Applications (1)

Application Number Title Priority Date Filing Date
PCT/US1993/012609 WO1995018353A1 (en) 1993-12-28 1993-12-28 Method and apparatus for monitoring thin films

Country Status (2)

Country Link
JP (1) JP3993888B2 (en)
WO (1) WO1995018353A1 (en)

Cited By (20)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
US6068539A (en) * 1998-03-10 2000-05-30 Lam Research Corporation Wafer polishing device with movable window
US6108091A (en) * 1997-05-28 2000-08-22 Lam Research Corporation Method and apparatus for in-situ monitoring of thickness during chemical-mechanical polishing
US6111634A (en) * 1997-05-28 2000-08-29 Lam Research Corporation Method and apparatus for in-situ monitoring of thickness using a multi-wavelength spectrometer during chemical-mechanical polishing
US6146242A (en) * 1999-06-11 2000-11-14 Strasbaugh, Inc. Optical view port for chemical mechanical planarization endpoint detection
US6146248A (en) * 1997-05-28 2000-11-14 Lam Research Corporation Method and apparatus for in-situ end-point detection and optimization of a chemical-mechanical polishing process using a linear polisher
US6319093B1 (en) 2001-02-06 2001-11-20 International Business Machines Corporation Chemical-mechanical polishing system and method for integrated spin dry-film thickness measurement
US6361646B1 (en) 1998-06-08 2002-03-26 Speedfam-Ipec Corporation Method and apparatus for endpoint detection for chemical mechanical polishing
US6489624B1 (en) 1997-07-18 2002-12-03 Nikon Corporation Apparatus and methods for detecting thickness of a patterned layer
US6514775B2 (en) 2001-06-29 2003-02-04 Kla-Tencor Technologies Corporation In-situ end point detection for semiconductor wafer polishing
US6570662B1 (en) 1999-05-24 2003-05-27 Luxtron Corporation Optical techniques for measuring layer thicknesses and other surface characteristics of objects such as semiconductor wafers
US6579149B2 (en) 2001-02-06 2003-06-17 International Business Machines Corporation Support and alignment device for enabling chemical mechanical polishing rinse and film measurements
US6628397B1 (en) 1999-09-15 2003-09-30 Kla-Tencor Apparatus and methods for performing self-clearing optical measurements
US6671051B1 (en) 1999-09-15 2003-12-30 Kla-Tencor Apparatus and methods for detecting killer particles during chemical mechanical polishing
US6806970B2 (en) 1998-04-21 2004-10-19 Hitachi, Ltd. Thin film thickness measuring method and apparatus, and method and apparatus for manufacturing a thin film device using the same
US6916225B2 (en) 2000-01-25 2005-07-12 Nikon Corporation Monitor, method of monitoring, polishing device, and method of manufacturing semiconductor wafer
US6930782B1 (en) 2003-03-28 2005-08-16 Lam Research Corporation End point detection with imaging matching in semiconductor processing
US6934040B1 (en) 1999-05-24 2005-08-23 Luxtron Corporation Optical techniques for measuring layer thicknesses and other surface characteristics of objects such as semiconductor wafers
KR100673880B1 (en) * 2000-07-20 2007-01-25 주식회사 하이닉스반도체 Apparatus for measuring thickness of metal layer by using optical method and Method for measuring thickness of metal layer using the same
US7169016B2 (en) 2005-05-10 2007-01-30 Nikon Corporation Chemical mechanical polishing end point detection apparatus and method
CN110617786A (en) * 2018-06-18 2019-12-27 凯斯科技股份有限公司 Pad monitoring device, pad monitoring system comprising same and pad monitoring method

Families Citing this family (5)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
US6479309B1 (en) * 2001-05-25 2002-11-12 Advanced Micro Devices, Inc. Method and apparatus for determining process layer conformality
US7312154B2 (en) * 2005-12-20 2007-12-25 Corning Incorporated Method of polishing a semiconductor-on-insulator structure
KR101138757B1 (en) * 2010-08-10 2012-04-24 삼성중공업 주식회사 Apparatus for measuring dry film thickness
JP2017075791A (en) * 2015-10-13 2017-04-20 富士通株式会社 Method and device
CN114234821A (en) * 2021-12-20 2022-03-25 南京大学 Membrane electrode thickness detection device and detection method

Citations (4)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
US3623813A (en) * 1967-12-21 1971-11-30 Balzers Patent Beteilig Ag Method for monitoring temperature variations of radiation-permeable substrates for supporting thin coatings applied by vacuum deposition
US4618262A (en) * 1984-04-13 1986-10-21 Applied Materials, Inc. Laser interferometer system and method for monitoring and controlling IC processing
US4998021A (en) * 1988-11-18 1991-03-05 Dainippon Screen Mfg. Co., Ltd. Method of detecting an end point of surface treatment
US5046849A (en) * 1987-06-23 1991-09-10 U.S. Philips Corporation Device having an exchangeable substrate sleeve for measuring layer thickness

Patent Citations (4)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
US3623813A (en) * 1967-12-21 1971-11-30 Balzers Patent Beteilig Ag Method for monitoring temperature variations of radiation-permeable substrates for supporting thin coatings applied by vacuum deposition
US4618262A (en) * 1984-04-13 1986-10-21 Applied Materials, Inc. Laser interferometer system and method for monitoring and controlling IC processing
US5046849A (en) * 1987-06-23 1991-09-10 U.S. Philips Corporation Device having an exchangeable substrate sleeve for measuring layer thickness
US4998021A (en) * 1988-11-18 1991-03-05 Dainippon Screen Mfg. Co., Ltd. Method of detecting an end point of surface treatment

Cited By (26)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
US6108091A (en) * 1997-05-28 2000-08-22 Lam Research Corporation Method and apparatus for in-situ monitoring of thickness during chemical-mechanical polishing
US6111634A (en) * 1997-05-28 2000-08-29 Lam Research Corporation Method and apparatus for in-situ monitoring of thickness using a multi-wavelength spectrometer during chemical-mechanical polishing
US6146248A (en) * 1997-05-28 2000-11-14 Lam Research Corporation Method and apparatus for in-situ end-point detection and optimization of a chemical-mechanical polishing process using a linear polisher
US6261155B1 (en) 1997-05-28 2001-07-17 Lam Research Corporation Method and apparatus for in-situ end-point detection and optimization of a chemical-mechanical polishing process using a linear polisher
US6621584B2 (en) 1997-05-28 2003-09-16 Lam Research Corporation Method and apparatus for in-situ monitoring of thickness during chemical-mechanical polishing
US6489624B1 (en) 1997-07-18 2002-12-03 Nikon Corporation Apparatus and methods for detecting thickness of a patterned layer
US6068539A (en) * 1998-03-10 2000-05-30 Lam Research Corporation Wafer polishing device with movable window
US6254459B1 (en) 1998-03-10 2001-07-03 Lam Research Corporation Wafer polishing device with movable window
US6806970B2 (en) 1998-04-21 2004-10-19 Hitachi, Ltd. Thin film thickness measuring method and apparatus, and method and apparatus for manufacturing a thin film device using the same
US6361646B1 (en) 1998-06-08 2002-03-26 Speedfam-Ipec Corporation Method and apparatus for endpoint detection for chemical mechanical polishing
US6654132B1 (en) 1999-05-24 2003-11-25 Luxtron Corporation Optical techniques for measuring layer thicknesses and other surface characteristics of objects such as semiconductor wafers
US7042581B2 (en) 1999-05-24 2006-05-09 Luxtron Corporation Optical techniques for measuring layer thicknesses and other surface characteristics of objects such as semiconductor wafers
US6570662B1 (en) 1999-05-24 2003-05-27 Luxtron Corporation Optical techniques for measuring layer thicknesses and other surface characteristics of objects such as semiconductor wafers
US6934040B1 (en) 1999-05-24 2005-08-23 Luxtron Corporation Optical techniques for measuring layer thicknesses and other surface characteristics of objects such as semiconductor wafers
US6488568B1 (en) 1999-06-11 2002-12-03 Lam Research Corporation Optical view port for chemical mechanical planarization endpoint detection
US6146242A (en) * 1999-06-11 2000-11-14 Strasbaugh, Inc. Optical view port for chemical mechanical planarization endpoint detection
US6671051B1 (en) 1999-09-15 2003-12-30 Kla-Tencor Apparatus and methods for detecting killer particles during chemical mechanical polishing
US6628397B1 (en) 1999-09-15 2003-09-30 Kla-Tencor Apparatus and methods for performing self-clearing optical measurements
US6916225B2 (en) 2000-01-25 2005-07-12 Nikon Corporation Monitor, method of monitoring, polishing device, and method of manufacturing semiconductor wafer
KR100673880B1 (en) * 2000-07-20 2007-01-25 주식회사 하이닉스반도체 Apparatus for measuring thickness of metal layer by using optical method and Method for measuring thickness of metal layer using the same
US6319093B1 (en) 2001-02-06 2001-11-20 International Business Machines Corporation Chemical-mechanical polishing system and method for integrated spin dry-film thickness measurement
US6579149B2 (en) 2001-02-06 2003-06-17 International Business Machines Corporation Support and alignment device for enabling chemical mechanical polishing rinse and film measurements
US6514775B2 (en) 2001-06-29 2003-02-04 Kla-Tencor Technologies Corporation In-situ end point detection for semiconductor wafer polishing
US6930782B1 (en) 2003-03-28 2005-08-16 Lam Research Corporation End point detection with imaging matching in semiconductor processing
US7169016B2 (en) 2005-05-10 2007-01-30 Nikon Corporation Chemical mechanical polishing end point detection apparatus and method
CN110617786A (en) * 2018-06-18 2019-12-27 凯斯科技股份有限公司 Pad monitoring device, pad monitoring system comprising same and pad monitoring method

Also Published As

Publication number Publication date
JP3993888B2 (en) 2007-10-17
JPH09511328A (en) 1997-11-11

Similar Documents

Publication Publication Date Title
US7024063B2 (en) In-situ real-time monitoring technique and apparatus for endpoint detection of thin films during chemical/mechanical polishing planarization
US7582183B2 (en) Apparatus for detection of thin films during chemical/mechanical polishing planarization
WO1995018353A1 (en) Method and apparatus for monitoring thin films
US5597442A (en) Chemical/mechanical planarization (CMP) endpoint method using measurement of polishing pad temperature
US5433650A (en) Method for polishing a substrate
US5705435A (en) Chemical-mechanical polishing (CMP) apparatus
US5643050A (en) Chemical/mechanical polish (CMP) thickness monitor
KR100368191B1 (en) Process for polishing a layer over a patterned semiconductor substrate
US5838448A (en) CMP variable angle in situ sensor
US5433651A (en) In-situ endpoint detection and process monitoring method and apparatus for chemical-mechanical polishing
KR100329891B1 (en) Chemical mechanical polishing in-situ end point system
US7042581B2 (en) Optical techniques for measuring layer thicknesses and other surface characteristics of objects such as semiconductor wafers
US6654132B1 (en) Optical techniques for measuring layer thicknesses and other surface characteristics of objects such as semiconductor wafers
KR20080090326A (en) Methods and apparatus for generating a library of spectra and high throughput measurement system
KR20010022689A (en) Method and apparatus for endpoint detection for chemical mechanical polishing
US6895360B2 (en) Method to measure oxide thickness by FTIR to improve an in-line CMP endpoint determination
US6437868B1 (en) In-situ automated contactless thickness measurement for wafer thinning
US20050118839A1 (en) Chemical mechanical polish process control method using thermal imaging of polishing pad
US5834375A (en) Chemical-mechanical polishing planarization monitor
US6309900B1 (en) Test structures for testing planarization systems and methods for using same
KR100555169B1 (en) Thin film inspection method
JP2002025960A (en) Method and apparatus for monitoring thin film
KR100304158B1 (en) Apparatus for monitoring thickness change in a film on substrate
KR100458700B1 (en) Method for monitoring thickness change in a film on substrate
JP2001284301A (en) Method and device monitoring thin film

Legal Events

Date Code Title Description
AK Designated states

Kind code of ref document: A1

Designated state(s): JP KR

AL Designated countries for regional patents

Kind code of ref document: A1

Designated state(s): AT BE CH DE DK ES FR GB GR IE IT LU MC NL PT SE

121 Ep: the epo has been informed by wipo that ep was designated in this application
DFPE Request for preliminary examination filed prior to expiration of 19th month from priority date (pct application filed before 20040101)
WWE Wipo information: entry into national phase

Ref document number: 1019960703512

Country of ref document: KR

122 Ep: pct application non-entry in european phase
WWE Wipo information: entry into national phase