WO2013134112A3 - Resistance welding process and method of control - Google Patents
Resistance welding process and method of control Download PDFInfo
- Publication number
- WO2013134112A3 WO2013134112A3 PCT/US2013/028843 US2013028843W WO2013134112A3 WO 2013134112 A3 WO2013134112 A3 WO 2013134112A3 US 2013028843 W US2013028843 W US 2013028843W WO 2013134112 A3 WO2013134112 A3 WO 2013134112A3
- Authority
- WO
- WIPO (PCT)
- Prior art keywords
- parts
- joined
- resistance welding
- control
- welding process
- Prior art date
Abstract
A method for resistance welding parts together is provided that includes the steps of clamping the parts to be joined together with electrodes; closing the gap between the parts to be joined; squeezing the parts together to deform contact surfaces on the parts to be joined; heating the parts to soften the material; monitoring the contact force between the parts; and forcing the parts together and upsetting material when the contact force reaches a predetermined value. It may also include the steps of holding the parts after being forced together and upset to reduce shrinkage stress and preheating the parts to increase the temperature before the heating cycle is commenced.
Applications Claiming Priority (2)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
US201261606760P | 2012-03-05 | 2012-03-05 | |
US61/606,760 | 2012-03-05 |
Publications (2)
Publication Number | Publication Date |
---|---|
WO2013134112A2 WO2013134112A2 (en) | 2013-09-12 |
WO2013134112A3 true WO2013134112A3 (en) | 2015-06-18 |
Family
ID=49117488
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
PCT/US2013/028843 WO2013134112A2 (en) | 2012-03-05 | 2013-03-04 | Resistance welding process and method of control |
Country Status (1)
Country | Link |
---|---|
WO (1) | WO2013134112A2 (en) |
Citations (5)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US4912295A (en) * | 1987-08-27 | 1990-03-27 | Sumitomo Metal Industries, Ltd. | Butt welding method |
US5880425A (en) * | 1997-04-29 | 1999-03-09 | Board Of Regents, The University Of Texas System | Method and apparatus for joining metals |
US20070131316A1 (en) * | 2003-10-22 | 2007-06-14 | Tadashi Ishikawa | Large-heat-input butt welded joints having excellent brittle fracture resistance |
US20090120919A1 (en) * | 2007-11-08 | 2009-05-14 | Lincoln Global, Inc. | Method of welding two sides of a joint simultaneously |
US20100108654A1 (en) * | 2008-11-03 | 2010-05-06 | Ulrich James F | Weld parameter interface |
-
2013
- 2013-03-04 WO PCT/US2013/028843 patent/WO2013134112A2/en active Application Filing
Patent Citations (5)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US4912295A (en) * | 1987-08-27 | 1990-03-27 | Sumitomo Metal Industries, Ltd. | Butt welding method |
US5880425A (en) * | 1997-04-29 | 1999-03-09 | Board Of Regents, The University Of Texas System | Method and apparatus for joining metals |
US20070131316A1 (en) * | 2003-10-22 | 2007-06-14 | Tadashi Ishikawa | Large-heat-input butt welded joints having excellent brittle fracture resistance |
US20090120919A1 (en) * | 2007-11-08 | 2009-05-14 | Lincoln Global, Inc. | Method of welding two sides of a joint simultaneously |
US20100108654A1 (en) * | 2008-11-03 | 2010-05-06 | Ulrich James F | Weld parameter interface |
Also Published As
Publication number | Publication date |
---|---|
WO2013134112A2 (en) | 2013-09-12 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
WO2010144931A8 (en) | Method for changing a welding process during a welding operation and method for applying heat prior to a welding operation | |
JP2016528044A5 (en) | ||
EP3566044A4 (en) | Apparatus and method for initiating thermal runaway in a battery | |
WO2013181141A8 (en) | Anisotropic porous scaffolds and method of making anisotropic porous scaffolds | |
WO2013140266A3 (en) | Applying rf energy according to time variations in em feedback | |
EP3542917A4 (en) | Operation monitoring device, method and program for high-frequency resistance welding and induction heated welding of electric resistance welded steel pipe | |
MX2017011826A (en) | Resistance spot welding method and method for manufacturing resistance spot welded joint. | |
MX2017016307A (en) | Mechanical bonding device and mechanical bonding method. | |
JP2016510261A5 (en) | ||
MX2015012678A (en) | Welded blank assembly and method. | |
ES2722406T3 (en) | Resistance welding in several stages of sandwich plates | |
WO2014113527A4 (en) | Methods for counteracting rebounding effects during solid state resistance welding of dissimilar materials | |
AU2013224000A8 (en) | Method and machine for forge welding of tubular articles and exothermic flux mixture and method of manufacturing an exothermic flux mixture | |
CN103084501A (en) | Local heating self-piercing riveting method for magnesium alloy plates | |
MX2017011757A (en) | Sonotrode for an ultrasound welding system and method for welding a connection element to a component. | |
WO2013134112A3 (en) | Resistance welding process and method of control | |
EP2979848A8 (en) | Thermoplastic joining system and method | |
WO2014041170A3 (en) | Method for pressing or welding the protective cover of a high temperature sensor | |
WO2014041166A3 (en) | High temperature sensor and method for producing a protective cover for a high temperature sensor | |
WO2015188800A3 (en) | Joining method | |
MX364566B (en) | Casting device and casting method. | |
WO2012165767A3 (en) | Secondary battery and method for fabricating same | |
MX2015013849A (en) | Terminal crimping device and terminal crimping method. | |
WO2016174474A3 (en) | Joining method | |
US20170239928A1 (en) | Device for hardening an electrically conductive adhesive |
Legal Events
Date | Code | Title | Description |
---|---|---|---|
121 | Ep: the epo has been informed by wipo that ep was designated in this application |
Ref document number: 13757158 Country of ref document: EP Kind code of ref document: A2 |
|
NENP | Non-entry into the national phase |
Ref country code: DE |
|
122 | Ep: pct application non-entry in european phase |
Ref document number: 13757158 Country of ref document: EP Kind code of ref document: A2 |